Product Details:
Payment & Shipping Terms:
|
Materials: | Duplex Steel UNS S32205/S31803 | Product Name: | Duplex Stainless Steel Tube |
---|---|---|---|
Standard: | ASME SA789 | O.D.: | 5/8"-2" |
W.T.: | BWG18-BWG14 | Length MAX: | 12000MM Max. |
Pipe Finish: | TIG Welded | Type: | Welded |
Shape: | Round | Surface: | Bright Annealed |
Application: | Heat Exchanger | Package: | Wooden Case |
High Light: | duplex stainless steel pipe,duplex ss pipe |
Duplex and Super duplex stainless steel USN31803/2205 Heat Exchanger Tube
The 2205 grade steel is one of the most widely used ferritic and austenitic duplex stainless steel. The standard of this grade of steel has been refined over the years creating a versatile and strong product. It is has an excellent corrosion resistance (including in seawater), it is weldable by all standard methods, and has a high heat resistance.
Features
Applications can be used in chemical processing, transport, and storage for a variety of industries due to both its excellent corrosion resistance and high strength.
Specifications:
UNS S31803
ASME SA-182 (F51), SA-240, SA-798, SA-790, SA-815
ASTM A182 (F51),A240, A276, A479, A789, A790, A815, A928, A988
SAE J405
UNS S32205
ASME SA-182 (F60), SA-240, SA-798, SA-790, SA-815
ASTM A182 (F60), A240, A276, A479, A480, A798, A790, A815, A928, A988
SAE J405
Specifications of Duplex Stainless Steel Welded Tube
1. Standard: ASTM ASME
2. Grade: 630 / 631 / 2205 / 2507 / 17-4PH
ASTM A789, ASTM A790, ASTM A450, ASTM A530,
GB/T 14976, GB/T 14975, GB/T 13296, etc
3. OD: 8mm-1000mm
4. Wall thickness: 0.3mm-30mm
5. Length: max.18000mm or as demand
6. Surface finish: Polishing (180#,220#,240#,320#400#,600#), Hairline, acid pickled, etc.
2205 is a duplex (austenitic-ferritic) stainless steel containing about 40 - 50% ferrite in the annealed condition. 2205 has been a practical solution to chloride stress corrosion cracking problems experienced with 304/304L or 316/316L stainless. The high chromium, molybdenum and nitrogen contents provide corrosion resistance superior to 316/316L and 317L stainless in most environments. 2205 is not suggested for operating temperatures above 600°F.
The design strength of 2205 is significantly higher than 316/316L, often permitting lighter wall construction. 2205 has good notch impact toughness down to temperatures below - 40°F. 2205 is welded with E2209 or ER2209 fillers.
Features
Specifications (ASTM/ASME) Duplex Stainless Steel Pipe | ||||
Alloy | UNS Designation | Material Specification |
Tubing Specification |
Pipe Specification |
2205 | S31803/S32205 | A 240/SA-240 | A 270 | A 790/SA-790 |
A 789/SA-789 | A928/SA928 |
Chemical Compositions:
Chemical Composition (%) Duplex Stainless Steel Pipe | ||
Alloy | 2205 | 2205 |
UNS Designation | S31803 | S32205 |
Carbon (C) max. | 0.030 | 0.030 |
Manganese (Mn) max. | 2.00 | 2.00 |
Phosphorus (P) max. | 0.030 | 0.030 |
Sulfur (S) max. | 0.020 | 0.020 |
Silicon (Si) max. | 1.00 | 1.00 |
Chromium (Cr) | 21.0 - 23.0 | 22.0 - 23.0 |
Nickel (Ni) | 4.5 - 6.5 | 4.5 - 6.5 |
Molybdenum (Mo) | 2.5 - 3.5 | 3.0 - 3.5 |
Nitrogen (N) | 0.08 - 0.20 | 0.14 - 0.20 |
Iron (Fe) | Balance | Balance |
Contact Person: Will Ma
Tel: +86 13918539222